Glassfiber Reinforced PP+20%GF
Product Detailed
Glassfiber Reinforced PP+20%GF
1.high rigidity,low stress
2.good chemical corrosivity resistance
3.excellent processing prop
Glassfiber Reinforced PP
1.introduction
Item | Drying temperature | Drying hours | Barrel temperature | Mold Temperature |
PP+20%GF | 70-90 | 4 | 190-250 | 40-70 |
2.main products:
----Dyeing ABS, PS, PMMA, AS, PC,PP plastic particles
----Dyeing ABS, PS, PP plastic particles of flame retardant, antibacterial, weather, anti-static, and pearl plush features
----Dyeing ABS, PC/ABS, PS, PP modified to enhance and mineral-filled
plastic particles